Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 200 kV/mm | 5080 kV/in | ASTM D149 |
Parker Chomerics T-Wings Heat Spreaders Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade.. |
|||
Dielectric Strength | 200 kV/mm @Thickness 0.0500 mm |
5080 kV/in @Thickness 0.00197 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Dielectric Strength | 200 kV/mm @Thickness 0.0500 mm |
5080 kV/in @Thickness 0.00197 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Dielectric Strength | 200 kV/mm | 5080 kV/in | 1/4 in electrode; ASTM D149 |
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled
(Unve Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Dielectric Strength | 200 kV/mm @Temperature 23.0 °C |
5080 kV/in @Temperature 73.4 °F |
1/4 inch electrode; ASTM D149 |
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application.. |
|||
Dielectric Strength | 200 kV/mm @Temperature 23.0 °C |
5080 kV/in @Temperature 73.4 °F |
1/4 inch electrode; ASTM D149 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Dielectric Strength | 200 kV/mm @Frequency 50.0 Hz, Temperature 150 °C |
5080 kV/in @Frequency 50.0 Hz, Temperature 302 °F |
DIN 40634 or VDE 0345 in air |
Mitsubishi Hostaphan® RN, 36 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Dielectric Strength | 200 kV/mm | 5080 kV/in | D.C. |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
Dielectric Strength | 200 kV/mm @Thickness 0.0500 mm |
5080 kV/in @Thickness 0.00197 in |
ASTM D149 |
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc.. |
|||
Dielectric Strength | 200 kV/mm @Thickness 0.0500 mm |
5080 kV/in @Thickness 0.00197 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Dielectric Strength | 200 kV/mm @Thickness 0.0500 mm |
5080 kV/in @Thickness 0.00197 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Dielectric Strength | 200 kV/mm | 5080 kV/in | 25 µm; ASTM D149 |
UBE UPILEX VT Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |
|||
Dielectric Strength | >= 200 kV/mm | >= 5080 kV/in | ASTM D149 |
CEN® Electronic Material CF 150CF019 Polyimide Film CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an.. |
|||
Dielectric Strength | >= 200 kV/mm | >= 5080 kV/in | ASTM D149 |
CEN® Electronic Material CF 200CF919 Polyimide Film CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an.. |
|||
Dielectric Strength | >= 200 kV/mm | >= 5080 kV/in | ASTM D149 |
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Dielectric Strength | >= 200 kV/mm | >= 5080 kV/in | ASTM D149 |
CEN® Electronic Material CF 120CF616 Polyimide Film CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an.. |
|||
Dielectric Strength | >= 200 kV/mm | >= 5080 kV/in | |
CEN® Electronic Material CN Polyimide Film, 1 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |