Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 5080 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 200 kV/mm
5080 kV/in
ASTM D149
Parker Chomerics T-Wings Heat Spreaders
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade..
Dielectric Strength 200 kV/mm

@Thickness 0.0500 mm
5080 kV/in

@Thickness 0.00197 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Dielectric Strength 200 kV/mm

@Thickness 0.0500 mm
5080 kV/in

@Thickness 0.00197 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Dielectric Strength 200 kV/mm
5080 kV/in
1/4 in electrode; ASTM D149
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled  (Unve
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Dielectric Strength 200 kV/mm

@Temperature 23.0 °C
5080 kV/in

@Temperature 73.4 °F
1/4 inch electrode; ASTM D149
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled
APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application..
Dielectric Strength 200 kV/mm

@Temperature 23.0 °C
5080 kV/in

@Temperature 73.4 °F
1/4 inch electrode; ASTM D149
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
Dielectric Strength 200 kV/mm

@Frequency 50.0 Hz,
Temperature 150 °C
5080 kV/in

@Frequency 50.0 Hz,
Temperature 302 °F
DIN 40634 or VDE 0345 in air
Mitsubishi Hostaphan® RN, 36 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin..
Dielectric Strength 200 kV/mm
5080 kV/in
D.C.
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..
Dielectric Strength 200 kV/mm

@Thickness 0.0500 mm
5080 kV/in

@Thickness 0.00197 in
ASTM D149
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc..
Dielectric Strength 200 kV/mm

@Thickness 0.0500 mm
5080 kV/in

@Thickness 0.00197 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Dielectric Strength 200 kV/mm

@Thickness 0.0500 mm
5080 kV/in

@Thickness 0.00197 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Dielectric Strength 200 kV/mm
5080 kV/in
25 µm; ASTM D149
UBE UPILEX VT Polyimide Film
Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries..
Dielectric Strength >= 200 kV/mm
>= 5080 kV/in
ASTM D149
CEN® Electronic Material CF 150CF019 Polyimide Film
CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an..
Dielectric Strength >= 200 kV/mm
>= 5080 kV/in
ASTM D149
CEN® Electronic Material CF 200CF919 Polyimide Film
CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an..
Dielectric Strength >= 200 kV/mm
>= 5080 kV/in
ASTM D149
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..
Dielectric Strength >= 200 kV/mm
>= 5080 kV/in
ASTM D149
CEN® Electronic Material CF 120CF616 Polyimide Film
CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an..
Dielectric Strength >= 200 kV/mm
>= 5080 kV/in
CEN® Electronic Material CN Polyimide Film, 1 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..
Copyright © lookpolymers.com All Rights Reserved