Product Description: HMA 016 is a HDPE grade, characterized by fast cycling and good impact strength. It has high gloss and high dimensional stability.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: YesUV Stabilizer: NoApplications: ClosuresFood Packaging ContainersHousewaresToysInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D4883
ESCR 10% Igepal® 2.0 hour

@Temperature 50.0 °C
2.0 hour

@Temperature 122 °F
F50; ASTM D1963
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3300 psi
ISO 527-2/1A/50
Elongation at Break >= 100 %
>= 100 %
ISO 527-2/1A/50
Elongation at Yield 10 %
10 %
ISO 527-2/1A/50
Flexural Modulus 0.896 GPa
130 ksi
ISO 178
Izod Impact, Notched (ISO) 4.20 kJ/m²
2.00 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point <= 266 °C
<= 511 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 66.1 °C
151 °F
ISO 75-2/B