Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.00 GPa | 725 ksi | |
Plastcom SLOVAMID 66 GF 20 HI PA66, 20% glass beads FeaturesChemically reinforced with 20% glass beeds, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Nilit FRIANYL A63 HH-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |
|||
Tensile Modulus | 5.00 GPa @Thickness 0.100 mm |
725 ksi @Thickness 0.00394 in |
MD; ISO 527 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
DSM Akulon® S223-PG2U (Dry) 13% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **)& Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
DSM Akulon® K224-TPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry)
(discontinued **)&l The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-3830 30% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-3830 is a 30% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3830 is recommended for producing in.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ASTM D638 |
Loxim 220 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WZ002 PBT LNP* THERMOCOMP* WZ002 is a compound based on PBT resin containing 10% Milled Glass. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MFK42AS PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFK42AS is a compound based on PP resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66 Information provided by A. Schulman. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 50mm/min; ISO 527-1 |
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Eurotec® Tecomid® NB40 MR30 NL PA 6 30% mineral reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-1/-2 |
DSM Akulon® S223-GM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ASTM D638 |
Aclo Accutech Polypropylene CP0435G43CV Copolymer Glass Reinforced Coupled Approved to GMP.PP.039 Black A13054 |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-2 |
CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used in high temperature applications. CENTROTRON has a low sliding friction coefficient and high abrasion resista.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ASTM Test |
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid B3GM35 BKQ642 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1mm/min; ISO 527 |
Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin GF 15% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527 |
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66 Information provided by A. Schulman. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1mm/min; ISO 527 |
BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Modulus | 5.00 GPa | 725 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p.. |