Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Eccobond® D 275 One-Component Fast Cure Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® D 275 One-Component Fast Cure Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy AdhesiveSemi-rigid, high strength, fast curing, pourable, epoxy structural adhesive. Good peel strength (12 pli), Recommended for bonding metals, plastics, and ceramics. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Viscosity 70000 cP

@Temperature 25.0 °C
70000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Adhesive Bond Strength 31.0 MPa
4500 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 6.00 min

@Temperature 160 °C
0.100 hour

@Temperature 320 °F
20.0 min

@Temperature 120 °C
0.333 hour

@Temperature 248 °F
60.0 min

@Temperature 100 °C
1.00 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Color Black