Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 31.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 31.0 MPa
4500 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Tra-Con Tra-Bond 216R01 Fire Retardant Epoxy
TRA-BOND 216R01 is a fast curing material with a set time of 5 to 7 minutes. Samples tested were certified to the requirements of UL94 V-O, and is RoHS compliant. TRA-BOND 216R01 develops significa..
Adhesive Bond Strength 31.0 MPa
4500 psi
Lap shear, alum to alum, @ 25°C
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive
TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s..
Adhesive Bond Strength 31.0 MPa
4500 psi
Trelleborg Emerson & Cuming Eccobond® D 275 One-Component Fast Cure Epoxy Adhesive
Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy AdhesiveSemi-rigid, high strength, fast curing, pourable, epoxy structural adhesive. Good peel strength (12 pli), Recommended for bond..
Adhesive Bond Strength 31.0 MPa
4500 psi
Steel/Steel; Varies with substrates
Loctite® 638 Maximum Strength Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Adhesive Bond Strength 31.0 MPa

@Temperature 82.2 °C
4500 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-701 Epoxy Adhesive
A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond..
Adhesive Bond Strength 31.0 MPa
4500 psi
Steel-Steel; after optimum cure
Armstrong C-7/W Epoxy Adhesive, 3:2 Mix Ratio
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
Adhesive Bond Strength 31.0 MPa
4500 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Tra-Con Tra-Bond FS411 Fast Cure Epoxy Adhesive System
TRA-BOND FS-411 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. It was designed to have low outgassing in ..
Copyright © lookpolymers.com All Rights Reserved