Polymer Property : Cure Time = 0.100 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 6.00 - 42.0 min

@Temperature 25.0 °C
0.100 - 0.700 hour

@Temperature 77.0 °F
De-mold Time
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer
MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th..
Cure Time 6.00 min

@Temperature 130 °C
0.100 hour

@Temperature 266 °F
Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System
Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interco..
Cure Time 6.00 min

@Temperature 160 °C
0.100 hour

@Temperature 320 °F
Trelleborg Emerson & Cuming Eccobond® D 275 One-Component Fast Cure Epoxy Adhesive
Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy AdhesiveSemi-rigid, high strength, fast curing, pourable, epoxy structural adhesive. Good peel strength (12 pli), Recommended for bond..
Cure Time 6.00 min

@Temperature 204 °C
0.100 hour

@Temperature 399 °F
3M Scotchcast™ 5230N Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moistu..
Cure Time 6.00 min

@Temperature 204 °C
0.100 hour

@Temperature 399 °F
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var..
Cure Time 6.00 min

@Temperature 177 °C
0.100 hour

@Temperature 351 °F
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin
3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating..
Cure Time 6.00 min

@Temperature 218 °C
0.100 hour

@Temperature 424 °F
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)
3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate..
Cure Time 6.00 min

@Temperature 218 °C
0.100 hour

@Temperature 424 °F
3M Scotchkote™ 412 Spray Grade Fusion Bonded Epoxy Coating
3M Scotchkote Spray Grade Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to pre..
Cure Time 6.00 min

@Temperature 140 °C
0.100 hour

@Temperature 284 °F
Dry to stack, at 50% humidity
Blue River Coatings Wood Primer
BLUE RIVER COATINGGS WOOD PRIMER is a high quality, single component primer, not requiring any catalyzing agent. WOOD PRIMER offers good coverage, excellent durability, and ease of application, as w..