Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon Fiber Reinforced
Manufacturer Teijin
Trade Name Panlite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applications:Mechanical, electric and electronic components that need stiffness and strengthMechanical, electric and electronic components that need extremely high dimensional accuracy.Mechanical, electric and electronic components that need electric conductivity or antistatic propertyInformation provided by Teijin Chemicals Ltd.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Water Absorption 0.16 %
0.16 %
in water, 23°C, 24h; ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm

@Thickness 4.00 mm
0.0010 - 0.0030 in/in

@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Thickness 4.00 mm
0.0040 - 0.0060 in/in

@Thickness 0.157 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
50mm/min; ISO 527
Elongation at Break 2.5 %
2.5 %
50mm/min; ISO 527
Tensile Modulus 7.70 GPa
1120 ksi
1mm/min; ISO 527
Flexural Strength 165 MPa
23900 psi
2mm/min; ISO 178
Flexural Modulus 7.40 GPa
1070 ksi
2mm/min; ISO 178
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ISO 75
Vicat Softening Point 152 °C
306 °F
50°C/hr, 50N; ISO 306
UL RTI, Electrical 80.0 °C

@Thickness 1.47 mm
176 °F

@Thickness 0.0579 in
UL 746B
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.47 mm
176 °F

@Thickness 0.0579 in
UL 746B
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 1.47 mm
176 °F

@Thickness 0.0579 in
UL 746B
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.0 - 100 ohm-cm
1.0 - 100 ohm-cm
IEC 60093
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
IEC 60093