Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.70 GPa | 1120 ksi | |
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 45% glass fibre, contains the modifier of mechanical properties.Thermo stable. Increased strength in comparison wit.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ISO 527-1,2 |
Qualchem Danamid FGFLX2-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | |
LATI Latigray 82-02 CX/80 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RX01075 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX01075 is a compound based on Nylon 66 resin containing PTFE, Mineral. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1mm/min; ISO 527 |
Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
Plenco 7203 Phenolic, Granular, Transfer Molded PLENCO 07203 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and an industrial finish. UL recognized under component file E40654. 07203 is available i.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MZ 301 CP Combination Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR 30% Glass Reinforced, Flame Retardant (Halogen free) |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Tensile Modulus | 7.70 GPa @Temperature -40.0 °C |
1120 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned) Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi.. |