Material Notes:
The ELI grade has lower impurity limits than standard titanium 6-4.Uses: applications requiring excellent fracture toughness and fatigue strength, aircraft, structural components, biomedical.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Physical Properties Metric English Comments
Density 4.43 g/cc
0.160 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 30
30
Tensile Strength, Ultimate 828 MPa
120000 psi
Tensile Strength, Yield 759 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
Elongation at Break 10 %
10 %
Component Elements Properties Metric English Comments
Aluminum, Al <= 6.5 %
<= 6.5 %
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.25 %
<= 0.25 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.13 %
<= 0.13 %
Titanium, Ti 90 %
90 %
as balance
Vanadium, V 4.0 %
4.0 %