Polymer Property : Izod Impact, Notched = 4.81 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.81 J/cm

@Temperature -40.0 °C
9.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Polymer Resources PC/TP-GP3 PC/Polyester Alloy
High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
9.00 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Techmer ES Plastiblend® PC/ABS 2110 BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
9.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® PC/PBT IM 6200 BK
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 4.81 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
9.01 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ABSPC 7030-HES ABS/PC Injection Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
9.01 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade
Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a..
Izod Impact, Notched 4.81 J/cm

@Temperature -20.0 °C
9.00 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP)
AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded..
Izod Impact, Notched 4.81 J/cm

@Thickness 6.35 mm,
Temperature -17.8 °C
9.00 ft-lb/in

@Thickness 0.250 in,
Temperature 0.000 °F
ASTM D-256
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 4.81 J/cm

@Thickness 6.35 mm,
Temperature -17.8 °C
9.00 ft-lb/in

@Thickness 0.250 in,
Temperature 0.000 °F
ASTM D-256
Axiall 7803 Rigid PVC, Extrusion High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.