Material Notes:
Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Linear Mold Shrinkage, Flow 0.0145 - 0.0185 cm/cm
0.0145 - 0.0185 in/in
Linear Mold Shrinkage, Transverse 0.0145 - 0.0185 cm/cm
0.0145 - 0.0185 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
Elongation at Break >= 100 %
>= 100 %
Elongation at Yield 4.5 %
4.5 %
Tensile Modulus 2.20 GPa
319 ksi
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Vicat Softening Point 130 °C

@Load 5.00 kg
266 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 200 - 240 °C
392 - 464 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa