Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.74 J/cm @Temperature -40.0 °C |
7.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/66 IM 6040 MB Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
7.00 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 7000 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 7000 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8003 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
7.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS 2110 BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
7.00 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall ProTherm® 4345 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4345 is a CPVC powder blend designed for extrusion applications requiring high heat deflection temperatures. Processing and stability along with overall physical properties .. |