Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 82.7 MPa @Thickness 3.17 mm |
12000 psi @Thickness 0.125 in |
ASTM D790 |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Ensinger ENSITEP® PBT Polybutylene Terephthalate - Extruded Products
(discontinued **) ENSITEP BT is an unreinforced thermoplastic polyester derived from polybutylene terephthalate. Its excellent wear and impact resistance, low coefficient of friction, high flexural modulus, and supe.. |
|||
Flexural Yield Strength | 82.7 - 131 MPa | 12000 - 19000 psi | Average value: 93.5 MPa Grade Count:35 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 82.7 - 178 MPa | 12000 - 25800 psi | Average value: 143 MPa Grade Count:7 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Plenco 4100 Phenolic, Granular, Compression Molded
(discontinued **) Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and .. |
|||
Flexural Yield Strength | 82.7 - 193 MPa | 12000 - 28000 psi | Average value: 151 MPa Grade Count:6 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 82.7 - 245 MPa | 12000 - 35500 psi | Average value: 126 MPa Grade Count:14 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Global GP-150 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Spartech SP-3010 Rigid PVC Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Star Plastics PC20NBR Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Luriblend® PC IM FR Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS 830 SS7 BK Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Statiblend® PC/ABS 830 SS7 BK with Stainless Steel Fiber Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Techmer ES Elastoblend® PC IM Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
PlastxWorld CEVIAN® DR210 PC Alloy High impact, good flowability and heat resistant.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Clariant Renol BR7008 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 82.7 - 134 MPa | 12000 - 19500 psi | Average value: 102 MPa Grade Count:7 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Yield Strength | 82.7 - 186 MPa | 12000 - 27000 psi | Average value: 121 MPa Grade Count:11 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Flexural Yield Strength | 82.7 - 276 MPa | 12000 - 40000 psi | Average value: 184 MPa Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Flexural Yield Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Styron PULSE™ EXT 100 PC/ABS Engineering Resin Overview: PULSE EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT 100 engin.. |
|||
Flexural Yield Strength | 82.7 - 176 MPa | 12000 - 25500 psi | Average value: 143 MPa Grade Count:12 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |