Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® ABS/PBT 1000

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® ABS/PBT 1000.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ASTM D638
Flexural Strength 72.4 MPa
10500 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C
211 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149