Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Spartech Centrex SP-6710 Weatherable Sheet Description: Weatherable SheetCentrex is a registered trademark of Bayer Corporation.Information provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Spartech EP5140 Talc Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food cont.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Spartech GELOY SP-6730 Weatherable Sheet Description: Weatherable SheetGeloy is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Spartech Royalite R570 FR-ABS Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | unannealed, .125in; ASTM D648 |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GB50 50% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPU 1000 Availability: North AmericaForms: PelletsFeatures: High DensityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | Unannealed; ASTM Data |
Styron Magnum™ 9015 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | Unannealed; ASTM D648 |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Chevron Phillips MC3700 High Flow Crystal Polystyrene DescriptionChevron polystyrene resin MC3700 crystal is a free-flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled or long-flow, difficult.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Americas Styrenics EB6400 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | ASTM D648 |
Americas Styrenics STYRON® 487R High Impact Polystyrene Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by Amer.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 °C | 175 °F | Unannealed; ASTM D648 |
M. Holland Company IS330 Polystyrene, High Impact
(discontinued **) Features: Impact ModifiedUses: Audio Tapes, Household Goods, ToysApprovals: FDA 21 CFR 177.1640Processing Method: Injection MoldingInformation provided by M. Holland. |