Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.08 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Multibase Multi-Pro® 2516 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Mytex Polymers AS65KWLGUS Polypropylene, Talc filled, Compounded
Description: Talc filled compounded polypropylene with high stiffness, superior impact balance, surface hardness and extremely low gloss.Key Applications: Non-painted instrument panelInformation pro..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
PolyOne OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
OnFlex™ U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™ U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Dow INSPIRE™ D7000 Thermoplastic Polyolefin  (discontinued **)
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line.
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792, ISO 1183
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792, ISO 1183
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6
Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au..
Density 1.08 g/cc
0.0390 lb/in³
DIN 53479
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane
Introduction: AVALON 60 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 ABX is part of the AVALON Perform Range and offers a specially designed,..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Asia Pacific)
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE. Added features of this material include: Internally Lubricated.
Density 1.08 g/cc
0.0390 lb/in³
ASTM D 792
Shakespeare Isocorâ„¢ 653 Nylon 6 Terpolymer
Isocorâ„¢ 653 multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ 653 is easily processed and has a wide range of applications due ..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D 792
Shakespeare Isocorâ„¢ TT65SI Nylon 6 Terpolymer
Isocorâ„¢ TT65SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Unlike conventional polyamides, Isocorâ„¢ TT65SI is soluble in common al..
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON CD000I PS
LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Styron EMERGEâ„¢ 5100 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5100 is a pre-colored, white, ABS resin, having high opacity and excellent toughness intended for manufacture of laser-marketable injection-molded smart cards.Information provided b..
Density 1.08 g/cc
0.0390 lb/in³
Solvay ALBRITECT® CP 30 Vinyl phosphonic acid - acrylic acid copolymer, 20% Aqueous solution
VINYL PHOSPHONIC ACID – ACRYLIC ACID COPOLYMER (20% SOLUTION IN WATER) CAS: 27936 – 88 – 5Solubility in Water: Miscible (in all proportions)Available in: Asia Pacific, Europe, Latin A..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP V1000UXC PA
LNP* Thermotuf* V1000UXC is a compound based on Nylon resin. Added features of this material include: UV Stabilized.
Density 1.08 g/cc
0.0390 lb/in³
Solvay MACKADET® EQ-178 Surfactant
Product Description: Mackadet EQ-178 is a mild, concentrated blend of surfactants for use as a base for high foam personal care products. This blend is free of alcohol, diethanolamides, lauryl sulfa..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East)
Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The ..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Styrolution Absolan® 2500 SAN
Absolac 2500 is a heat and chemical resistant gradeInformation provided by Styrolution
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Polyram PlusTek PA862 Nylon 6.6 for Injection Molding, High Impact Modified
High impact modified Nylon 6.6 for injection molding applications.Information provided by Polyram.
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Tipco Tipcolene® NPI 200 IN - 25% Talc/Mineral Reinforced Polypropylene Copolymer with Very High Flow, Stiffness & Impact Strength
20% Mineral Reinforced, Very High Stiffness & Very High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries ..
Density 1.08 g/cc
0.0390 lb/in³
Trelleborg Emerson & Cuming Stycast® 1265 Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
Density 1.08 g/cc
0.0390 lb/in³
Loctite® 243 Oil Resistant/Medium Strength Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
Density 1.08 g/cc
0.0390 lb/in³
EMS-Griltech Grilon® XA 136 Nylon 610 Monofilament (Super-Set)
Description: GRILON XA 136 is a Nylon 610 based monofilament for paper machine, clothing, forming screen, and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provid..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
EMS-Grivory Grivory® CF 7 PA*
Product description Grilon CF 7 is a Copolyamide. Good flexibility and toughnessGood thermoforming and orientation propertiesGood shrink characteristicsGood transparencyReduced melting point Grilon ..
Density 1.08 g/cc
0.0390 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, Conditioned
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry)
Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o..
Density 1.08 g/cc
0.0390 lb/in³
Solvay RHODAPEX® ESC-70/AB Surfactant
Chemical Name: Sodium Laureth SulfateCAS: 68585-34-2Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX ESC-70/AB is used in the formulation of high quality sh..