Techmer ES Plaslube® J-1/AF/10/TF/10/HS BL8816 PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Aramid Fiber Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-1/AF/10/TF/10/HS BL8816 PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.70 %
0.70 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100 - 110
100 - 110
ASTM D785
Tensile Strength at Break 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256