Mechanical Properties Metric English Comments
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether
Description: Norpex® AX20MR is a 20% mineral reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Res..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Electrafil® NY-7/EC NAT PA6
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES HiFill® PEI BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES HiFill® PEI HF BK
Availability: North AmericaForms: PelletsFeatures: High FlowAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES HiFill® PEI TX5 LE
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Low Extractables and LubricatedInformation provided by TP Composites, Inc.
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 AF10 HS L Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Low Fric..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 AF10 Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionInformation provided by..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Plaslube® J-1/AF/10/TF/10/HS BL8816 PA66
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Plaslube® J-1/AF/15/TF/10 NAT PA66
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Statiblend® PBT 03003
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass FiberFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Composites, Inc.
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES Statiblend® PBT GF10 SS5 MB
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: AntistaticFeatures: Conductive, Antistatic and ESD ProtectionInformation provided by TP Comp..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
PlastxWorld CEVIAN® CGF20 20% GF PC/Acrylic Alloy
Glass fiber reinforced PC/Acrylic alloy.These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc.
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Chase Plastics CP Pryme® PC110R Polycarbonate, 10% Glass Fiber Reinforced
Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics.
Flexural Modulus 3.52 GPa
510 ksi
Tangent; ASTM D790
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Chesterton ARC 10 Paste grade machinable composite
Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Ensinger Tecatron® XP-78 Compression Molded PPS Compound, 47% PTFE Filled Seal Material
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Flexural Modulus 3.52 GPa
510 ksi
Abatron AboCast 8502-5/AboCure 8502-5 Colorless, Low-Exotherm Epoxy Casting Compound
AboCast 8502-5/AboCure 8502-5 is a rigid, colorless, low-exotherm epoxy casting compound for spherical masses up to 500 grams. It is a 2-component structural and dielectric liquid system with extrem..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Asahi Kasei Thermylene® P6-20FG-0753 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Chesterton MRS 10 Metal Rebuilding System
Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 10..
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Techmer ES HiFill FR® PPO/HIPS MM20 FR 20% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by Weight Features: Flame RetardantInformation provided by TP Composites, Inc.