Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 124 MPa | 18000 psi | ASTM D-790 |
Plaskolite Optix® CA - 87 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 124 - 154 MPa | 18000 - 22300 psi | ASTM D790 |
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi.. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
PolyOne Edgetek® AS-30GF/000 FRVO Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 124 MPa | 18000 psi | |
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially.. |
|||
Flexural Strength | 124 - 145 MPa | 18000 - 21000 psi | ASTM D790 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES Electrablend® PPS 06000 Availability: North AmericaForms: PelletsFiller/Reinforcement: Metallic FlakeFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 124 MPa | 18000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 457 PBT 6.5% GR PBT, UL94 V-0/5V. |
|||
Flexural Strength | 124 MPa | 18000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES HiFill® PA6 CM30 HS BK 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInf.. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES HiFill® PA6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composit.. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES Plaslube® J-1/AF/15/TF/10 NAT PA66 |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2949 PPE+PS (Asia Pacific) PPE+PS GF+Mineral Filler total 40% |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF002XXP Acetal Copoly LNP* Thermocomp* KF002XXP is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Flexural Strength | 124 MPa | 18000 psi | ISO 178 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Flexural Strength | 124 MPa | 18000 psi | ISO 178 |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Flexural Strength | 124 MPa | 18000 psi | |
BCC Products BC 5008-2 General Purpose Epoxy System BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A.. |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
Techmer ES Luriblend® HTN 01410 BK Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant and Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppear.. |
|||
Flexural Strength | 124 MPa @Temperature 22.8 °C |
18000 psi @Temperature 73.0 °F |
ASTM D790 |
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide |
|||
Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
PolyOne Edgetek® AT-25GF-10MN/000 NATURAL Acetal-Copolymer, Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 124 MPa | 18000 psi | |
XXXPC Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |