Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Water Absorption 0.60 %
0.60 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 131 MPa
19000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 197 MPa
28500 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Compressive Strength 193 MPa
28000 psi
ASTM D695
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256