Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6 PA6 GR20 IM6 Glass Reinforced/Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2033STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
PolyOne Edgetek® ATH-10CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
PolyOne Edgetek® AS-13CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
PolyOne Edgetek® BB-20GF/000 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 6.21 - 28.3 GPa | 900 - 4100 ksi | Average value: 13.8 GPa Grade Count:44 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF18 FR BK 18% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Plaslube® J-50/20/TF/15 Polycarbonate, 20% Glass Reinforced, PTFE Lubricated 20% Glass Reinforced, PTFE Lubricated |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Chase Plastics CP Pryme® N120GL (DAM) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Ensinger XP-133 Compression Molded PI Compound, 20% Carbon Fiber The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 6.21 - 7.58 GPa | 900 - 1100 ksi | |
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
PolyOne Edgetek® AT-25GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |