Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 193 MPa | 28000 psi | |
Ohio Carbon Blank OCB TTK-4C EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
IDI Composites A-205 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
IDI Composites M-106 Thermoset Polyester, Molding Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer. |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
IDI Composites M-205 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Compressive Strength | 193 MPa | 28000 psi | |
Haysite 42000 Polyester SMC, 22% Glass Reinforced The 42000 series sheet molding compound is an electrical grade designed for compression molded parts requiring high strength and good electrical properties. This material possesses excellent moldabi.. |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
Techmer ES Plaslube® J-1/20/TF/20 BK PA66 |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
Techmer ES Plaslube® J-1/30/TF/22 BK223 PA66 |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
Techmer ES Plaslube® J-1/30/TF/22 NAT PA66 |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Compressive Strength | 193 MPa | 28000 psi | |
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Compressive Strength | 193 MPa | 28000 psi | |
Cosmic Plastics E487 lass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Compressive Strength | 193 MPa | 28000 psi | |
Cosmic Plastics E4930 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Compressive Strength | 193 MPa | 28000 psi | 90° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Compressive Strength | 193 MPa | 28000 psi | 10% Deformation; ASTM D695 |
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Compressive Strength | 193 MPa | 28000 psi | |
3M iM30K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Compressive Strength | 193 - 207 MPa | 28000 - 30000 psi | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Compressive Strength | 193 - 228 MPa | 28000 - 33000 psi | |
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Compressive Strength | 193 - 228 MPa | 28000 - 33000 psi | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Compressive Strength | >= 193 MPa | >= 28000 psi | Break; TM R050-38 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Compressive Strength | >= 193 MPa | >= 28000 psi | Ultimate; TM R050-38 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Compressive Strength | >= 193 MPa | >= 28000 psi | Break; TM R050-38 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Compressive Strength | >= 193 MPa | >= 28000 psi | Ultimate; TM R050-38 |
Resinlab® EP1026R Rubber Modified Epoxy Adhesive Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free .. |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
Resinoid 1324 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
Plenco 7579 Phenolic, Granular, Compression Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
Compressive Strength | 193 MPa | 28000 psi | ASTM D695 |
Sumitomo Bakelite North America FM 1132P Cellulose Reinforced Phenolic Novolac FM 1132P is a two-stage phenolic molding compound reinforced with cellulose in pellet form. FM-1132P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-10. (Replaces Militar.. |
|||
Compressive Strength | 193 MPa @Strain 10.0 %, Temperature 22.8 °C |
28000 psi @Strain 10.0 %, Temperature 73.0 °F |
ASTM D695 |
Quadrant EPP Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide |
|||
Compressive Strength | 193 MPa | 28000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |
|||
Compressive Strength | >= 193 MPa | >= 28000 psi | Ultimate; TM R050-38 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Compressive Strength | >= 193 MPa | >= 28000 psi | Break; TM R050-38 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |