Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP521-188 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9777 Medium Beige Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 23.0 °C |
1.70 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-5001 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | 0.125 in, 73°F; ASTM D256 |
Matrixx Group 80S7451 45% Glass Reinforced PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS BLACK PPE/Nylon Alloy 30% Glass Filled Information provided by PTS LLC. |
|||
Izod Impact, Notched | 0.908 - 4.97 J/cm | 1.70 - 9.30 ft-lb/in | Average value: 2.10 J/cm Grade Count:60 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4702-8 Polycarbonate EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi.. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 22.8 °C |
1.70 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene GPP1630 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 30% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Teknor Apex Synres® SR 4321 Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Izod Impact, Notched | 0.908 J/cm @Thickness 3.17 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® LMW48 Laser Markable Grade ABS White MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive) Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated.. |
|||
Izod Impact, Notched | 0.908 J/cm @Temperature 0.000 °C |
1.70 ft-lb/in @Temperature 32.0 °F |
ASTM D256A |
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions.Formolene 6502A is a medium impact copolymer with an excellent balance of t.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | 73°F; ASTM D256 |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | |
Asahi Kasei Thermylene® P7-20FG-0876 Chemically Coupled Polypropylene Compound, 20% Glass Filled Applications: Automotive: Sun Roof Rails, Fan Shrouds, Air Cleaners, Battery Boxes, Air Induction Components, Battery Trays, Blower Wheels, Light Housings, Shifter Bases, Interior Consoles, Arm Rest.. |