Techmer ES HiFill® PA6/6 HS N MB Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized , Nylon 66, Nucleated
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 HS N MB Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Lubricant, Nucleating Agent and Heat StabilizerFeatures: Lubricated, Fast Molding Cycle, Nucleated and Heat StabilizedTPCI# 8384101Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 2.90 GPa
420 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 77.4 µm/m-°C
43.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 237 °C
459 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149