Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers SAN 280 Water Clear Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |
Quadrant EPP PROTEUS® EURO-GRAY Copolymer Polypropylene |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Annealed; ASTM D648 |
Network Polymers NPS 80-0800 Crystal Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
M. Holland Company IS410 Polystyrene, High Impact
(discontinued **) Features: Good Colorability, High Flow, Impact ModifiedUses: Household Goods, Modeling Material, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Annealed (2 hours @ 176°F); ASTM-D648 |
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |
Techmer ES Electrafil® DB-1200/SS/7 ABS, 7% Stainless Steel Fiber Reinforced (dry blend) Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 HS N MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant, Nucleating Agent and Heat StabilizerFeatures: Lubricated, Fast Molding Cycle, Nucleated and Heat StabilizedTPCI# 8384101Information prov.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |
Techmer ES Plaslube® NY-1/TF/10 Nylon 66, 10% PTFE Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C @Thickness 3.20 mm |
190 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HIPS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® LDPE 0098 S LE Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Heat StabilizerFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM Test |
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry) Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® NN100M2HS (Dry) Nylon 66, Lubricated, Heat Stabilized Features: Good chemical resistanceFast cycleDurableHeat stabilizedLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPS 100-1 GPPS BLACK Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A reprocessed, general-purpose Polystyrene resin, compounded black, specifically designed for all high speed injection molding appli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | |
Aclo Accutech Polypropylene Copolymer CP0436G10CL Glass Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |
Asahi Kasei Thermylene® F6-10FG-0100 10% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | |
BCC Products BC 5010 Epoxy Laminating System BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor.. |