Techmer ES HiFill® PA6/6 G/CF20 IM HS BK 20% GlassCarbon Filler

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Carbon Fiber Filled , Nylon 66, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 G/CF20 IM HS BK 20% GlassCarbon Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 131 MPa
19000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
490 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10000 - 1.00e+7 ohm-cm
10000 - 1.00e+7 ohm-cm
ASTM D257
Surface Resistance 10000 - 1.00e+7 ohm
10000 - 1.00e+7 ohm
ASTM D257
Users viewing this material also viewed the following: