Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
ASTM D648
Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized
Nylon 66, 33% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
ASTM D648
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
ASTM D648
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed, 0.125 in bars; ASTM D648
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp  (discontinued **)<
Information provided by PolyOne™ Corporation
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N1020HL BK Nylon 6/6  (discontinued **)
Available in North America Filler: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedForm: Pellets Processing Method: I..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N1030HL Nylon 6/6  (discontinued **)
Available in North America Filler: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: GM GMW3038P-PA..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 G/CF20 IM HS BK 20% GlassCarbon Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 GF20 HS BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 GF20 HS L 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformati..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 GF20 HS L BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA6/6 GF20 L BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced
Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
ASTM D648
Ensinger HYDLAR® Z Nylon, Pultruded Aramid Fiber Reinforced (PA)
HYDLAR® possesses a combination of physical properties that cannot be found in any other commercially available engineered plastic. Design engineers have created a family of superior wear and abra..
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
ASTM D648
Clariant Renol 6608G33HSL Nylon 66, 33% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated