Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+7 ohm @Thickness 2.00 mm |
1.00e+6 - 1.00e+7 ohm @Thickness 0.0787 in |
sheet; IEC 61340-5-1 |
Panipol Oy DXH-PP Inherently Conductive Polymer Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are contr.. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D4496 |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+7 ohm @Thickness 2.00 mm |
1.00e+6 - 1.00e+7 ohm @Thickness 0.0787 in |
sheet; IEC 61340-5-1 |
Panipol Oy DXH Inherently Conductive Polymer Panipol DXH composition is conductive masterbatch for melt processing with commodity polymers such as polypropylene. It is based on doped and plasticized Polyaniline. Benefits of Panipol DXH grade.. |
|||
Surface Resistance | 10.0 - 1.00e+7 ohm | 10.0 - 1.00e+7 ohm | Average value: 797000 ohm Grade Count:21 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | Average value: 1.20e+6 ohm Grade Count:10 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
Surface Resistance | 10.0 - 1.00e+7 ohm | 10.0 - 1.00e+7 ohm | Average value: 2.59e+6 ohm Grade Count:12 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | IEC 60093 |
LG Chemical LUCON CP6052 PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi.. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC LNP STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Clean Compounding System. Easy Molding, Electrically Conductive. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC (Asia Pacific) LNP* STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX01303C PC LNP STAT-KON* DX01303C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC (Asia Pacific) LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
Techmer ES HiFill® PA6/6 G/CF20 IM HS BK 20% GlassCarbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp.. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
Techmer ES HiFill® PA6/6 G/CF30 L BK 30% GlassCarbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp.. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66 LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Surface Resistance | 100 - 1.00e+7 ohm | 100 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific) LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
Techmer ES Electrablend® PA6 GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Surface Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX92002 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX92002 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 100 - 1.00e+7 ohm | 100 - 1.00e+7 ohm | Average value: 1.84e+6 ohm Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Surface Resistance | 1.00 - 1.00e+7 ohm | 1.00 - 1.00e+7 ohm | Average value: 363000 ohm Grade Count:43 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Surface Resistance | 1000 - 1.00e+7 ohm | 1000 - 1.00e+7 ohm | ASTM D257 |
PolyOne Lubri-Tech™ MP-15MCF/15T-2S Modified PPO - 15% Milled Carbon Fiber - 15% PTFE - 2% Silicone
(disconti Data provided by PolyOne. |