Electrical Properties Metric English Comments
Volume Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
400 um thick sheet; ISO D-257
Premix Thermoplastics PRE-ELEC® PE 1291
PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Volume Resistivity <= 10000 ohm-cm

@Thickness 0.400 mm
<= 10000 ohm-cm

@Thickness 0.0157 in
ISO D-257
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
IEC 93
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific)
LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Volume Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
ISO D-257
Premix Thermoplastics PRE-ELEC® CP 1318  (discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Stainless Steel Reinforcement, 13/10% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation..
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc.
Volume Resistivity 10000 - 1.00e+8 ohm-cm
10000 - 1.00e+8 ohm-cm
ASTM D257
Techmer ES HiFill® PA6 0137 S2
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+PS
LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall.
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Techmer ES Luriblend® PC CF10 TL10 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I..
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
conditioned; IEC 60093
EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30
Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties: high stiff..
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
IEC 60093
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black
Information provided by Eurotec®
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Adamas Adalon® 125 PTFE, 35% Carbon Filled
Information provided by Adamas, HPM
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Adamas Adalon® 139 PTFE, 35% Soft Carbon Filled
Information provided by Adamas, HPM
Volume Resistivity 10000 - 1.00e+6 ohm-cm
10000 - 1.00e+6 ohm-cm
ASTM D 257
SABIC Innovative Plastics LNP Verton OX07411 PPS
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Copyright © lookpolymers.com All Rights Reserved