| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled |
| Manufacturer | Techmer ES |
| Trade Name | HiFill® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES HiFill® PA6 GF50 X 50% Glass Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.58 g/cc | 0.0571 lb/in³ | ASTM D792 |
| Water Absorption | 0.75 % <br>@Time 86400 sec |
0.75 % <br>@Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm <br>@Thickness 3.17 mm |
0.0020 in/in <br>@Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 121 | 121 | ASTM D785 |
| Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
| Elongation at Break | 2.5 % | 2.5 % | ASTM D638 |
| Flexural Strength | 324 MPa | 47000 psi | ASTM D790 |
| Flexural Modulus | 14.1 GPa | 2050 ksi | ASTM D790 |
| Izod Impact, Notched | 1.87 J/cm <br>@Thickness 3.17 mm |
3.50 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Unnotched | 11.2 J/cm <br>@Thickness 3.17 mm |
21.0 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 14.4 µm/m-°C | 8.00 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 218 °C | 425 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Strength | 17.7 kV/mm | 450 kV/in | Method A (Short-Time); ASTM D149 |