Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 221 MPa | 32100 psi | ASTM D638 |
PolyOne OnForce™ LFT UR-40 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | |
Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1000-25All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated Iron FX-226-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1000-25Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Tensile Strength, Yield | 221 MPa @Temperature 23.9 °C |
32000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ES-40CF/000 Polyethersulfone - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Tensile Strength, Yield | 221 MPa @Thickness 3.20 mm |
32000 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 221 MPa @Strain 0.200 %, Temperature 538 °C |
32100 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 221 MPa @Strain 0.200 %, Temperature 760 °C |
32100 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 CF40 40% Carbon Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAppearance: Black and Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 L LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: Natural ColorInf.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP C.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 X 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 X LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | |
TriStar TriSteel PE Metal Backed PTFE Bearing System Ultraflon 603 PE lined metal backed bearing system, with or without lube, high PV, high temperature... Ultraflon 603 PE Liner is a bearing grade polymer for use in lubricated or unlubricated environ.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 221 MPa | 32100 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade Made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Tensile Strength, Yield | 221 MPa | 32100 psi | ASTM D638 |
Ashley Polymers Ashlene® 528L-50G Nylon 66, 50% Glass Reinforced A general purpose 50% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 221 MPa @Strain 0.200 % |
32100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 11 Titanium (UNS R52250) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | 221 MPa @Strain 0.200 %, Temperature 649 °C |
32100 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |