Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PC SS10 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: ConductiveInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF40 L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF40 RM HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer Features: Heat Stabilized and Low Moisture AbsorptionAppearanc.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF44 HS L 44% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 44% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized TPCI# 95.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF44 HS X 44% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 44% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized TPCI# 95.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 L BN047 LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: BeigeInformation.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 L LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: Natural ColorInf.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 X LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Com.. |
|||
Izod Impact, Unnotched | 11.2 J/cm @Thickness 3.17 mm |
21.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® PC FR BK Availability: North AmericaForms: PelletsAntistaticFeatures: Flame Retardant and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Izod Impact, Unnotched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 11.2 J/cm | 21.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |