Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 221 MPa | 32000 psi | |
Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1000-25All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated Iron FX-226-T Powdered Metal Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1000-25Information Provided by Pacific Sintered Metals, a division of PSM Ind.. |
|||
Tensile Strength, Yield | 221 MPa @Temperature 23.9 °C |
32000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ES-40CF/000 Polyethersulfone - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Tensile Strength, Yield | 221 MPa @Thickness 3.20 mm |
32000 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 CF40 40% Carbon Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAppearance: Black and Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizerInformati.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 L LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: Natural ColorInf.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP C.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 X 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 X LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | |
TriStar TriSteel PE Metal Backed PTFE Bearing System Ultraflon 603 PE lined metal backed bearing system, with or without lube, high PV, high temperature... Ultraflon 603 PE Liner is a bearing grade polymer for use in lubricated or unlubricated environ.. |
|||
Tensile Strength, Yield | 221 MPa | 32000 psi | ASTM D638 |
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber Data provided by Clariant Masterbatches |