Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 50H1 PA66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 50H1 PA66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phosphorus and halogen free flame retardant grade, offers excellent filling qualities combined with good stiffness. It is particularly suitable for molding insulating parts for electrical components: Components for electrical connections: junction blocks, terminal blocks, and connectors. This product is available in natural. Other colors can be provided upon requestInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
ISO 527 Type 1A
Tensile Strength, Yield 53.0 MPa
7690 psi
ISO 527 type 1 A
Elongation at Break 140 %
140 %
ISO 527 Type 1A
Elongation at Yield 22.3 %
22.3 %
ISO 527 type 1 A
Tensile Modulus 2.20 GPa
319 ksi
ISO 527 Type 1A
Flexural Strength 61.0 MPa
8850 psi
ISO 178
Flexural Modulus 1.71 GPa
248 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.01 J/cm²
4.81 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %