Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP66UT108 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY8540 PC+ABS (Europe-Africa-Middle East) CYCOLOY CY8540 is a PC+ABS blend, especially designed for textile backmolding in automotive interior applications. High flow grade, which allows low temperature processing to maintain fabric integri.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7647 PC Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer containing Graphite. Added features include : Internally Lubricated. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific) LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7680 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.0 MPa | 7680 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 53.0 MPa | 7680 psi | ASTM D638 |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL N190HF PPE+HIPS (Asia Pacific) |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | chs 5 mm/min; ASTM D638 |
Diamond Polymers ABSPC 7330-1801H ABS/PC Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 2 in/min; ASTM Test |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa | 7690 - 8270 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO value at 50 mm/min. |
BASF Capron® 8351 HS BK-102 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8351 HS BK-102 is a heat stabilized, pigmented black type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughness combined with a moderate fle.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML1661 PC Copolymer (Asia Pacific) Medium-flow impact-modified light-shielding high-flow-ductile PC copolymer. Available in white color only. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL EX130 PPE+HIPS (Asia Pacific) PPE+PS Auto Exterior Grade |