Formosa Plastics Formolon® 622S PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 622S PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer Siding Grade Resin F622S is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications, but it is also suitable for many flexible applications. This product has high bulk density and excellent dry flow characteristics, making it desirable for dry blending applications where uniform feed rate to an extruder is important.Applications: Siding, Calendering, Film, Rigid Profile and Rigid Expanded Profile. ASTM Classification: GP4-16000, ASTM D1755Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D1895
Volatiles 0.30 %
0.30 %
ASTM D6980
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
200 Mesh
200 Mesh
3% thru; Malvern
Viscosity 0.90 cP
0.90 cP
Inherent; ASTM D5225
Relative Viscosity 2.15 cP
2.15 cP
Descriptive Properties Value Comments
Color -0.2
a
1.8
b
97.5
L
Composition 2.0 ppm
Residual VCM, GC Head Space Method
20
Contamination Count, OCS per 100g
K-Value 65
Fikentscher's Constant