Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1.71 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.71 GPa
248 ksi
ASTM D790
Nylene® PA6/6 Impact Modified 311 HS Nylon 6/6
Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Flexural Modulus 1.71 GPa
248 ksi
ASTM D790
Nylene® PA6/6 Impact Modified 4114 HS Nylon 6/6
High Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Flexural Modulus 1.71 GPa
248 ksi
ASTM D790M
DSM Somos® 7110 Epoxy Photopolymer, Green Parts  (discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
Flexural Modulus 1.71 GPa

@Temperature 23.0 °C
248 ksi

@Temperature 73.4 °F
ASTM D790A
Ineos H02C-00 Polypropylene Homopolymer
This is a low flow rate, high clarity homopolymer designed for extrusion, thermoforming, blow molding, and rigid packaging. Applications that require good see-through clarity combined with good hea..
Flexural Modulus 1.71 GPa
248 ksi
ISO 178
Solvay TECHNYL® A 50H1 PA66, Conditioned
Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho..
Flexural Modulus 1.71 GPa
248 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp ML002S PP
LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the..
Flexural Modulus 1.71 GPa
248 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP
LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Flexural Modulus 1.71 GPa
248 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP QL004 PA6.10
LNP* LUBRICOMP* QL004 is a compound based on Nylon 6/10 containing 20% PTFE. Added features of this grade include: Wear Resistant.
Flexural Modulus 1.71 GPa
248 ksi
Tangent; ASTM D790
Plastics Group Polifil® 627L Nylon 6/6 (DAM)
Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group...
Flexural Modulus 1.71 GPa
248 ksi
ASTM D790
Diamond Polymers NYLON 6615 HS Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.