Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially developed additives, the product offers a good electrical conductivity, combined with a good dimensional stability.Available in: Latin AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: It is mostly used for fuel or oil filters.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527 Type 1A
Elongation at Break 10 %
10 %
ISO 527 Type 1A
Tensile Modulus 3.20 GPa
464 ksi
ISO 527 Type 1A
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²
3.09 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved