DuPont™ Appeel® 20D828 Ethylene Acrylate

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer DuPont
Trade Name Appeel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Appeel® 20D828 Ethylene Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temperature range to a number of container materials including PP, PS, PP, PVC, Aclar®, Barex®, and certain epoxy coatings. Appeel® 20D828 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Appeel® 20D828 Lidding Sealant Resin complies with Food and Drug Administration Regulation 21 CFR 175.320 – Resinous and polymeric coatings for polyolefin films, subject to the limitations and requirements therein. This regulation describes resinous and polymeric coatings for polyolefin films that may be used in contact with food under Conditions of Use C through H (as described in Table 2 of 21 CFR 176.170(c), subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (c ) of the Regulation.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792, ISO 1183
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 97.0 °C
207 °F
ASTM D3418, ISO 3146
Vicat Softening Point 58.0 °C
136 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 240 °C
<= 464 °F
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
160 °C
320 °F
Extrusion Coating
Zone 2 150 °C
302 °F
Blown Film Coextrusion
185 °C
365 °F
Extrusion Coating
Zone 3 160 °C
320 °F
Blown Film Coextrusion
210 °C
410 °F
Extrusion Coating
Zone 4 180 °C
356 °F
Blown Film Coextrusion
235 °C
455 °F
Extrusion Coating
Zone 5 180 °C
356 °F
Blown Film Coextrusion
235 °C
455 °F
Extrusion Coating
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
235 °C
455 °F
Extrusion Coating
Die Temperature 170 °C
338 °F
Blown Film Coextrusion
235 °C
455 °F
Extrusion Coating
Melt Temperature 150 - 190 °C
302 - 374 °F
Blown Film Coextrusion
180 - 240 °C
356 - 464 °F
Extrusion Coating
Dry Time 5.00 hour

@Temperature 55.0 °C
5.00 hour

@Temperature 131 °F
Users viewing this material also viewed the following: