Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid

Category Fluid , Polymer
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name Galden®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature ranges, are available. Uses include heat transfer, electronic reliability testing, vapor phase soldering, solvents, and acid spill mitigation.
Physical Properties Metric English Comments
Density 1.77 g/cc

@Temperature 25.0 °C
0.0639 lb/in³

@Temperature 77.0 °F
Solubility of Water 0.0014 %
0.0014 %
Kinematic Viscosity 1.8 cSt

@Temperature 25.0 °C
1.8 cSt

@Temperature 77.0 °F
3.41 cSt

@Temperature 0.000 °C
3.41 cSt

@Temperature 32.0 °F
7.11 cSt

@Temperature -20.0 °C
7.11 cSt

@Temperature -4.00 °F
21.14 cSt

@Temperature -40.0 °C
21.14 cSt

@Temperature -40.0 °F
Molecular Weight 760 g/mol
760 g/mol
average
Vapor Pressure 0.00107 bar

@Temperature 25.0 °C
0.800 torr

@Temperature 77.0 °F
Surface Tension 18 dynes/cm
18 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 66.9 J/g

@Temperature 170 °C
28.8 BTU/lb

@Temperature 338 °F
at boiling point
CTE, linear 367 µm/m-°C
204 µin/in-°F
converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C
Specific Heat Capacity 0.960 J/g-°C
0.229 BTU/lb-°F
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Boiling Point 170 °C
338 °F
Maximum Service Temperature, Air 170 °C
338 °F
as heat transfer fluid
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
as heat transfer fluid
Pour Point <= -97.0 °C
<= -143 °F
Optical Properties Metric English Comments
Refractive Index 1.281
1.281
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
Dielectric Constant 1.9

@Frequency 1000 Hz
1.9

@Frequency 1000 Hz
Dielectric Strength 15.7 kV/mm
399 kV/in
2.54 mm gap
Dissipation Factor 0.00020

@Frequency 1000 Hz
0.00020

@Frequency 1000 Hz
Descriptive Properties Value Comments
Solubility of Air (cm³ gas / 100 cm³ liquid) 26