Physical Properties Metric English Comments
Surface Tension 18 dynes/cm
18 dynes/cm
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Surface Tension 18 dynes/cm
18 dynes/cm
Dow Corning ST Cyclomethicone 5-NF
Volatile silicone, decamethylcyclopentasiloxane (Cyclomethicone NF) for use in a wide range of skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning
Surface Tension 18 dynes/cm
18 dynes/cm
Dow Corning XIAMETER® PMCPPMX-0245 Cyclopentasiloxane
Is chemically equivalent to DOW CORNING® 245 FLUID. This product a volatile, low viscosity cyclopentasiloxane fluid for use in skincare, suncare, color cosmetics, hair care, and antiperspirant / de..
Surface Tension 18 dynes/cm
18 dynes/cm
3M Fluorinert™ FC-70 Electronic Liquid
Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a..
Surface Tension 18 dynes/cm
18 dynes/cm
3M Novec™ Flux Remover
3M™ Novec™ Flux Remover is a strong, non-flammable cleaner ideal for removal of a wide variety of solder fluxes used in electronic manufacturing and repair - including rosin-based and many no-clea..
Surface Tension 18 dynes/cm
18 dynes/cm
3M Novec™ 72DA Engineered Fluid
3M™ Novec™ 72DA is ideal for flux removal and vapor degreasing operations. It is non-flammable and low in toxicity which makes it an ideal replacement for chlorinated solvents such as Trichloroeth..