Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -35.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Recommended
Nye Lubricants 701-EPS (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Recommended
Nye Lubricants 795A (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Recommended
Nye Lubricants UniFlor 8170R (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Recommended
Nye Lubricants UniFlor 8172R (829RP) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Precision Polymer Engineering N65H Nitrile Rubber
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content = 40% plus. Copolymer of acrylonitrile and butadiene.Applications: The high acrylonitrile content of this compound inc..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Precision Polymer Engineering N80E Nitrile Rubber
High Nitrile Rubber, 73-83 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. Aerospace Material Specification DTD5509..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Minimum temperature without fracturing after immersion in fluids
Precision Polymer Engineering N80E Nitrile Rubber
High Nitrile Rubber, 73-83 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. Aerospace Material Specification DTD5509..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering N90B Nitrile Rubber
General purpose, Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM & ISO designation = NBR. ASTM D2000 line call-out: M4CH910, A25, B14, EF31, EO15, EO35, F16.Applications..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering Q70B Polyurethane Rubber
Peroxide cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering Q70R Polyurethane Rubber
Peroxide cured, red Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion r..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering Q70Y Polyurethane Rubber
Peroxide cured, yellow Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering Q75B Polyurethane Rubber
Sulphur cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG728, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering Q80Y Polyurethane Rubber
Peroxide cured, yellow Polyurethane Rubber, 75-85 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG814, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering Q90B Polyurethane Rubber
Peroxide cured, Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Precision Polymer Engineering C90B Chloroprene Rubber
Chloroprene Rubber, 86-95 °IRHD. To meet British Standard BS5176 line call-out M2BC907.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleu..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Freudenberg Simrit V115 Standard Fluoroelastomer
Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Retraction Temperature, TR10; ASTM D1329
Seals Eastern 7346 Extreme Low Temperature Service Rubber
HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern.
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
as heat transfer fluid
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg B571 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg B574 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg E850 EPDM Rubber
EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and ..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg Hypalon® H511 Chlorosulphonated Polyethylene
PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing ..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg Hypalon® H608 Chlorosulphonated Polyethylene
PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing ..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg Hypalon® H611 Chlorosulphonated Polyethylene
PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing ..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene
PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing ..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg B870 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Trelleborg Hypalon® H606 Chlorosulphonated Polyethylene
PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing ..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
See Note 1.
ChevronTexaco MCP Grease L NLGI Grade 00
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
JIS-K-6723
Denka REOMER G G5379 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Brittleness Temperature
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (disco
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
Copyright © lookpolymers.com All Rights Reserved