Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | calculated |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | calculated |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Specific Heat Capacity | 0.960 - 1.03 J/g-°C @Temperature 0.000 - 50.0 °C |
0.229 - 0.246 BTU/lb-°F @Temperature 32.0 - 122 °F |
Average value: 0.995 J/g-°C Grade Count:1 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT135 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | Product Property; E1461-01 |
Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg.. |
|||
Specific Heat Capacity | 0.960 J/g-°C | 0.229 BTU/lb-°F | |
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem.. |