Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Asia Pacific) Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Europe-Africa-Middle East) Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Solvay Specialty Polymers Galden® HT135 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCD891B PPE-TPE Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Tra-Con Tra-Bond 7560D Hydrolytically Stable Adhesive TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product i.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Dow Corning 732 MULTI-PURPOSE SEALANT General-purpose acetoxy RTV sealantInformation provided by Dow Corning |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Dow Corning HV 1551/70P 40 Shore hardness low viscosity injection mouldable liquid silicone rubber with high tear strength, high elongation and a fast cure speed.Information provided by Dow Corning |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Dow Corning SE 9184 WHITE RTV One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Dow Corning 3-4190 SILICONE GEL KIT Two-part, transparent green, RT or heat cure, low viscosity, long shelf life.Information provided by Dow Corning |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | 50% RH; ASTM D-257 |
Axiall 17890 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for THW and 90C Class 43 applications. UL recognized component for THW and TW.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | 50% RH; ASTM D-257 |
Axiall 19900 Wire & Cable Flexible PVC 105°C; VW-1 rated non-lead stabilized insulation with good flexibility. Ideally suited for 1/64 wall (18 AWG and larger). UL approved for TW, THW, THHW applications.Information provided by Georgi.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | 50% RH; ASTM D-257 |
Axiall 19930 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | ASTM D257 |
3M 7959MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | 50% RH; ASTM D-257 |
Axiall 19482 Wire & Cable Flexible PVC 105°C, VW-1 rated non-lead stabilized insulation compound. Ideally suited for 18 AWG, 1/64 wall. UL approved for TW, THW, THHW applications.Information provided by Georgia GulfGeorgia Gulf became.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | ASTM D257 |
3M 9059MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | IEC 93 |
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab.. |
|||
Volume Resistivity | 1.50e+15 ohm-cm | 1.50e+15 ohm-cm | |
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem.. |