Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 170 °C | 338 °F | at 760 mmHg |
LyondellBasell PNB Propylene glycol normal butyl ether Information provided by Lyondell. |
|||
Boiling Point | <= 170 °C | <= 338 °F | End |
Kazanorgsintez E-8 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Boiling Point | 170 °C | 338 °F | |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Boiling Point | 170 °C | 338 °F | |
BASF Monoethanolamine Pure Formula: C2H7NOCAS: 141-43-5Description: Monoethanolamine pure is a colorless to yellow liquid with a perceptible amine-like odor. It is miscible with water.Synonyms: MEOA, 1-Amino-2-hydroxyethane,.. |