Kinematic Viscosity 21.14 cSt

@Temperature -40.0 °C
21.14 cSt

@Temperature -40.0 °F
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..