Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
50 mm/min; ASTM D638
Flexural Strength 36.3 MPa
5260 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.97 GPa
286 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.18 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C

@Thickness 6.40 mm
163 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 84.0 °C
183 °F
B/50; ISO R306
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in