Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
PolyMirae Moplen EP500N Injection Molding Grade Polypropylene Moplen EP500N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP500N is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
Reliance Industries Repol C015EG Polypropylene REPOL Polypropylene C015EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | ASTM D638 |
M. Holland Company CP420 Polypropylene Impact Copolymer AntistaticImpact copolymerGood impact resistanceLow temperature impact resistanceNucleatedApplications: Fishing applicationsFurnitureTool/tote box |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Hyosung Topilene R200P PP R200P Extrusion Random CopolymerApplications:Underfloor heating pipeWater service pipeCharacteristics:Pressure resistanceHigh impactLong-term heat stabilityFlexibilityInformation provided by Hyosung.. |
|||
Tensile Strength, Yield | 26.5 MPa @Thickness 3.20 mm |
3840 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Tensile Strength, Yield | 26.5 MPa @Thickness 3.20 mm |
3840 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer Features: SEETEC M1600 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1600 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC M1700 Polypropylene Impact Copolymer Features: SEETEC M1700 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1700 exhibits a very high flowability and a good balance of stiffness and impact strength.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical SEETEC PB270 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical SEETEC PH162 HDPE Features: Characteristics : Good balance of toughness & stiffness stressAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 200-230°C (392-446°C) f.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC R3400 Polypropylene Random Copolymer Features: Seetec R3400 is a polypropylene-ethylene random copolymer designed for non-transparent injection molding application. SEETEC R3400 meets the FDA requirement in the code of Federal Regulati.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC R3420 Polypropylene, Random Copolymer Features: Seetec R3420 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical SI-610 Alphalac Polystyrene High flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include big size electric app.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene HB6200 is a high density polyethylene for blow molding. HB6200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applic.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical 40 AF Flame Retardant HIPS High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical 60HR-G HIPS High flow, Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape reco.. |
|||
Tensile Strength, Yield | 26.5 MPa @Thickness 3.20 mm |
3840 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HM5001 High density polyethylene HM5001 is a high density polyethylene for yarn extrusion. HM5001 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2aApplic.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Tipco Tipcolene® FPZ-GC - Talc/Mineral Reinforced Polypropylene Copolymer, High Flow, Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | |
Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | |
Zylog Hipolyene® 9011 UHF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |