3M FV022902 Soft White Vinyl Label Product

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FV022902 Soft White Vinyl Label Product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Soft White Vinyl Label Product FV22902 is a flexible vinyl label stock that offers excellent durability and some moisture resistance. This vinyl label utilizes 3M™ Adhesive F2201 which is a freezer grade acrylic that offers high initial tack, good clarity, and adhesion when applied at temperatures as low as 0°F (-18°C) and also has excellent processing characteristics and offers exceptional adhesion to a wide variety of substrates with moderate resistance to water and humidity.Information provided by 3M
Physical Properties Metric English Comments
Thickness 78.7 microns
3.10 mil
Liner
88.9 microns
3.50 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
60.0 °C
140 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
-18.0 °C
-0.400 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type F2201 Freezer 16
Appearance 50# SC